Polyester Film Thermal Conductivity Technical Data
Polyester film thermal conductivity data are meaningful only when PET grade, film thickness, heat-flow direction, temperature, and retained layers are identified. This reference covers bare BOPET and defined adhesive-coated PET constructions used in insulation, converting, and temporary surface protection. Published values can support preliminary layer-resistance calculations; coated assemblies, heated processes, and removal behavior should be confirmed with samples on the intended surface and equipment.
The Measurement Boundary
This technical data sheet covers unfilled biaxially oriented PET base films, treated PET carriers, and defined adhesive-coated constructions used for through-thickness calculations.
It does not rate solar control, flammability, melting point, or universal service temperature. Resin, thick sheet, filled, metallized, and finished laminates need structure-matched data.
Thermal conductivity describes heat flow through the tested construction. For phase-transition behavior instead of heat-flow measurement, review polyester film DSC melting data. Keep thickness, temperature, and construction details with the conductivity result.
What Is Inside the Tested Stack
A test stack may contain PET base film, surface treatment, adhesive, and liner. Every retained layer must be identified so an assembly result is not mistaken for bare PET.
Treatment on corona-treated PET film supports coating anchorage, not a conductivity value. If PET release liner constructions remain attached, their carrier, silicone layer, and interfaces add resistance. Modified grades require separate confirmation.
Data Record for the Tested Construction
Replace reference entries with tested-grade or project-confirmed data when available.
Item | Typical Value / Reference Range | Test Method or Condition | Notes |
Base film | Identified industrial PET / BOPET grade | Construction record | State unfilled, treated, coated, or modified. |
Film construction | Bare PET or PET + treatment + adhesive + optional liner | Layer record | List all retained test layers. |
Film thickness | Project-confirmed, um | Calibrated gauge, multiple points | Report mean and range. |
Total construction thickness | Project-confirmed, um | Coating-compatible gauge | Do not replace with carrier thickness. |
Thermal conductivity | About 0.13-0.16 W/(m.K), unfilled BOPET reference | Through-plane near ambient; method stated | Confirm grade, direction, and temperature. |
Mean test temperature | Project-confirmed | Record hot and cold surfaces | Ambient data may not predict heated use. |
Calculated resistance | R'' = t/k, m2.K/W | Measured thickness and tested conductivity | Applies only to the identified layer. |
Surface treatment | Untreated, corona, or chemical | Identify treated side | Match test and production specimens. |
Adhesive type | Project-confirmed system | Construction record | Affects resistance and aged peel. |
Peel adhesion | Sample-specific | Defined substrate, dwell, angle, speed, temperature | Not a universal removal prediction. |
Tensile / elongation | Tested grade, MD and TD | ASTM D882, ISO 527-3, or equivalent | Supports handling and tear review. |
Haze / transmission | Tested clear construction | ASTM D1003 or equivalent | Optical values do not determine conductivity. |
Storage condition | Controlled indoor storage; intact packaging | Grade instruction | Recheck aged or exposed rolls. |
Choosing the Measurement Route
When one PET layer is too thin for stable measurement, test several layer counts under identical pressure and temperature. Plot resistance against total thickness: the slope estimates material resistivity, while the intercept reflects contact effects. Report thickness, pressure, replicates, regression quality, and uncertainty.
For coated film, define whether the result represents the PET carrier or the supplied assembly; report the latter as total resistance or apparent conductivity.
Test Item | What It Checks | Suggested Method or Reference | Why It Matters | When To Request It |
Through-plane conductivity | Heat across thickness | ISO 22007-2 or equivalent | Primary direction for film layers. | When heat flow affects design. |
Stacked-film resistance | Resistance across layer counts | ASTM E1530-type approach | Separates thickness and contact effects. | When one layer is too thin. |
In-plane conductivity | Heat along MD or TD | Validated anisotropic method | Checks orientation effects. | When lateral spreading matters. |
Thickness | Carrier and coated thickness | Multipoint calibrated gauge | Captures coat and cross-web variation. | For every comparison. |
Peel adhesion | Removal force after dwell | ASTM D3330, FINAT FTM 1, or equivalent | Depends on surface and settings. | For the actual coated surface. |
Dwell inspection | Lifting, bubbles, trace, gloss, tearing, residue | 24 h, 72 h, and 7 day comparison | Links data to surface behavior. | Before a new surface or process. |

From Conductivity to Layer Resistance
Polyester film thermal conductivity is a material property; thickness creates resistance. Under unchanged grade, direction, and temperature, 100 um film has about twice the PET-layer resistance of 50 um film. Low conductivity alone does not make an ultrathin film an effective insulator.
Thickness tolerance, adhesive coat weight, liner status, and contact resistance may outweigh small differences among published values. Data for flame-retardant polyester film should not replace unfilled PET data. Mechanical and optical properties cannot substitute for thermal measurement.
Where the Same Film Gives a Different Outcome
On glass, cleanliness, coatings, sunlight, and bubbles affect results. On metal, oil, texture, forming stress, and removal temperature matter. For electrical insulation PET film, review conductivity with dielectric needs, operating temperature, thickness, and the assembled heat-flow path.
Plastics differ in surface energy and additive migration. Painted surfaces need confirmed cure; rough surfaces trap air; low-energy surfaces may provide weak holding force.
Evidence from 24 h, 72 h and 7 Day Checks
Apply a representative sample using intended pressure or equipment settings. Record substrate, coating, temperature, humidity, orientation, and removal direction.
At 24 h, inspect peel, bubbles, distortion, and edge lifting. At 72 h, check adhesion build, trace, surface shadow, and gloss. At 7 days, check difficult removal, tearing, transfer, discoloration, coating interaction, and residue. Cool heated samples under intended conditions before removal.
Project samples may use verified film coating, slitting and quality-control capabilities, but records must identify the actual equipment or laboratory. Repeat testing when the surface, temperature, storage history, equipment, or operator changes.

Failure Signals Hidden by a Single Data Point
The table links data shifts to process symptoms and verification.
Data Point | If Too Low | If Too High | Risk in Application | Check Before Full Use |
Film thickness | Understates resistance; raises tear risk. | Raises resistance or stiffness. | Wrong heat estimate or handling. | Measure the actual roll. |
Thermal conductivity | Slower heat flow than calculated. | Faster heat flow than calculated. | Wrong temperature or process time. | Test grade, direction, and temperature. |
Peel adhesion | Lifting or poor wet-out. | Difficult removal or trace. | Protection failure or rework. | Run staged peel checks. |
Tensile / elongation | Splitting or low strain tolerance. | Stiffness, necking, or unstable peel. | Web break or incomplete removal. | Test MD and TD under intended tension. |
Surface treatment | Poor coating or adhesive anchorage. | Aged or excessive treatment inconsistency. | Delamination or uneven peel. | Identify side; confirm surface energy. |
Storage age / exposure | Performance below tested state. | Adhesion or optical change rises. | Lab-to-production mismatch. | Repeat peel, edge, and optical checks. |
Keeping the Reference Roll Comparable
Store rolls in intact packaging indoors, away from sunlight, moisture, condensation, dust, and heat. Prevent flattening, telescoping, core damage, and marked outer layers.
Long storage, hot transport, temperature cycling, or packaging damage can alter results. Equilibrate rolls before opening and repeat peel, edge, and residue checks after abnormal exposure.

Questions Raised During Technical Review
What is a typical polyester film thermal conductivity value?
Published values for unfilled BOPET are commonly about 0.13-0.16 W/(m.K) near ambient temperature. Treat this as a reference unless grade, direction, temperature, and method match.
Does thickness change conductivity or thermal resistance?
For a uniform grade, thickness changes layer resistance, not intrinsic conductivity. Coatings, interfaces, orientation, additives, and temperature can change the assembly result.
Can bare PET data be used for adhesive-coated protective film?
Only for a preliminary PET-layer estimate. Adhesive, treatment, liner, air gaps, and interfaces require validation of the complete construction.
Why are 24 h, 72 h, and 7 day checks necessary?
Adhesion develops over time. Staged checks reveal lifting, bubbles, trace, gloss change, difficult removal, tearing, or residue not visible immediately.